*24500$aEvaluation of decay of painted systems for wood, steel and galvanized steel after 4 years exposure$cJan F. Henriksen ... [et al.] ; prepared by the Sub-Centre for Painted Materials, Norwegian Institute for Air Research
*260 $aLillestrøm$bThe Institute$c1993
*300 $a41 s.$bdiagr.
*4901 $aNILU OR$v24/93
*4901 $aReport / UN/ECE International Co-operative Programme on Effects on Materials, including Historic and Cultural Moments$v14
*653 $alangtransportert$aluftforurensning$asur$anedbør$aoppløsning$amaling$atreverk$agalvanisert$astål$_270823900
*7001 $aHenriksen, J.F.$0(NO-TrBIB)90578280$_16317100
*830 0$aNILU OR (trykt utg.)$x0807-7207$v24/93$w998821280274702201$_13468400
*830 0$aReport (UN/ECE International Co-operative Programme on Effects on Materials, Including Historic and Cultural Monuments : trykt utg.)$v14$w999327226014702201$_28558900
*901 $a80
*999 $aoai:nb.bibsys.no:999327243704702202$b2021-11-14T20:50:36Z$z999327243704702202
^